سینٹرڈ NdFeB مقناطیس
sintered NdFeB مقناطیس جسمانی خصوصیات | ||||||||
گریڈ | باقیات | Rev. Temp.- Coeff. کے Br | زبردستی قوت | اندرونی جبر کی قوت | Rev. Temp.- Coeff. Hcj کے | زیادہ سے زیادہ توانائی کی مصنوعات | زیادہ سے زیادہ آپریٹنگ درجہ حرارت | کثافت |
Br (KGs) | ایچ سی بی (آپ) | Hcj (آپ) | (BH) زیادہ سے زیادہ (MGOe) | g/cm³ | ||||
N35 | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥12 | -0.58~-0.78 | 33-36 | 80℃ | 7.6 |
N38 | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥12 | -0.58~-0.78 | 36-39 | 80℃ | 7.6 |
N40 | 12.5-12.8 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 38-41 | 80℃ | 7.6 |
N42 | 12.8-13.2 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 40-43 | 80℃ | 7.6 |
این 45 | 13.2-13.8 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 43-46 | 80℃ | 7.6 |
N48 | 13.8-14.2 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 46-49 | 80℃ | 7.6 |
N50 | 14.0-14.5 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 48-51 | 80℃ | 7.6 |
N52 | 14.3-14.8 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 50-53 | 80℃ | 7.6 |
N33M | 11.3-11.7 | -0.11~-0.12 | ≥10.5 | ≥14 | -0.58~-0.72 | 31-33 | 100℃ | 7.6 |
N35M | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥14 | -0.58~-0.72 | 33-36 | 100℃ | 7.6 |
N38M | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥14 | -0.58~-0.72 | 36-39 | 100℃ | 7.6 |
N40M | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥14 | -0.58~-0.72 | 38-41 | 100℃ | 7.6 |
N42M | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥14 | -0.58~-0.72 | 40-43 | 100℃ | 7.6 |
N45M | 13.2-13.8 | -0.11~-0.12 | ≥12.5 | ≥14 | -0.58~-0.72 | 43-46 | 100℃ | 7.6 |
N48M | 13.6-14.3 | -0.11~-0.12 | ≥12.9 | ≥14 | -0.58~-0.72 | 46-49 | 100℃ | 7.6 |
N50M | 14.0-14.5 | -0.11~-0.12 | ≥13.0 | ≥14 | -0.58~-0.72 | 48-51 | 100℃ | 7.6 |
N35H | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥17 | -0.58~-0.70 | 33-36 | 120℃ | 7.6 |
N38H | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥17 | -0.58~-0.70 | 36-39 | 120℃ | 7.6 |
N40H | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥17 | -0.58~-0.70 | 38-41 | 120℃ | 7.6 |
N42H | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥17 | -0.58~-0.70 | 40-43 | 120℃ | 7.6 |
N45H | 13.2-13.6 | -0.11~-0.12 | ≥12.1 | ≥17 | -0.58~-0.70 | 43-46 | 120℃ | 7.6 |
N48H | 13.7-14.3 | -0.11~-0.12 | ≥12.5 | ≥17 | -0.58~-0.70 | 46-49 | 120℃ | 7.6 |
N35SH | 11.7-12.2 | -0.11~-0.12 | ≥11.0 | ≥20 | -0.56~-0.70 | 33-36 | 150℃ | 7.6 |
N38SH | 12.2-12.5 | -0.11~-0.12 | ≥11.4 | ≥20 | -0.56~-0.70 | 36-39 | 150℃ | 7.6 |
N40SH | 12.5-12.8 | -0.11~-0.12 | ≥11.8 | ≥20 | -0.56~-0.70 | 38-41 | 150℃ | 7.6 |
N42SH | 12.8-13.2 | -0.11~-0.12 | ≥12.4 | ≥20 | -0.56~-0.70 | 40-43 | 150℃ | 7.6 |
N45SH | 13.2-13.8 | -0.11~-0.12 | ≥12.6 | ≥20 | -0.56~-0.70 | 43-46 | 150℃ | 7.6 |
N28UH | 10.2-10.8 | -0.11~-0.12 | ≥9.6 | ≥25 | -0.52~-0.70 | 26-29 | 180℃ | 7.6 |
N30UH | 10.8-11.3 | -0.11~-0.12 | ≥10.2 | ≥25 | -0.52~-0.70 | 28-31 | 180℃ | 7.6 |
N33UH | 11.3-11.7 | -0.11~-0.12 | ≥10.7 | ≥25 | -0.52~-0.70 | 31-34 | 180℃ | 7.6 |
N35UH | 11.8-12.2 | -0.11~-0.12 | ≥10.8 | ≥25 | -0.52~-0.70 | 33-36 | 180℃ | 7.6 |
N38UH | 12.2-12.5 | -0.11~-0.12 | ≥11.0 | ≥25 | -0.52~-0.70 | 36-39 | 180℃ | 7.6 |
N40UH | 12.5-12.8 | -0.11~-0.12 | ≥11.3 | ≥25 | -0.52~-0.70 | 38-41 | 180℃ | 7.6 |
N28EH | 10.4-10.9 | -0.105~-0.120 | ≥9.8 | ≥30 | -0.48~-0.70 | 26-29 | 200℃ | 7.6 |
N30EH | 10.8-11.3 | -0.105~-0.120 | ≥10.2 | ≥30 | -0.48~-0.70 | 28-31 | 200℃ | 7.6 |
N33EH | 11.3-11.7 | -0.105~-0.120 | ≥10.5 | ≥30 | -0.48~-0.70 | 31-34 | 200℃ | 7.6 |
N35EH | 11.7-12.2 | -0.105~-0.120 | ≥11.0 | ≥30 | -0.48~-0.70 | 33-36 | 200℃ | 7.6 |
N38EH | 12.2-12.5 | -0.105~-0.120 | ≥11.3 | ≥30 | -0.48~-0.70 | 36-39 | 200℃ | 7.6 |
N28AH | 10.4-10.9 | -0.105~-0.120 | ≥9.9 | ≥33 | -0.45~-0.70 | 26-29 | 230℃ | 7.6 |
N30AH | 10.8-11.3 | -0.105~-0.120 | ≥10.3 | ≥33 | -0.45~-0.70 | 28-31 | 230℃ | 7.6 |
N33AH | 11.3-11.7 | -0.105~-0.120 | ≥10.6 | ≥33 | -0.45~-0.70 | 31-34 | 230℃ | 7.6 |
نوٹ: · کام کرنے والے درجہ حرارت 20℃±2℃ کے تحت، اوپر کے مقناطیسی پیرامیٹرز اور طبعی خصوصیات کی جانچ کی جاتی ہے، جس میں مقناطیسی قوت کا ناگزیر نقصان 5% سے زیادہ نہیں ہوتا۔ مقناطیس کا زیادہ سے زیادہ کام کرنے کا درجہ حرارت لمبائی اور قطر اور ماحولیاتی عوامل کے تناسب کی وجہ سے تبدیل ہوتا ہے۔ . |
فائدہ:
ان میگنےٹس کی خصوصیات روایتی سے کہیں زیادہ ہیں اور یہ فی الحال استعمال میں سب سے زیادہ طاقتور ہیں۔ ان کا اعلیٰ
جبر اور اعلی بحالی نئے ڈیزائن اور اطلاق کے مقناطیسی میدان میں اضافہ کے امکان کی اجازت دیتی ہے جہاں جگہ محدود ہے
یا جہاں ایک مضبوط مقناطیسی میدان کی ضرورت ہے۔
NdFeB میگنےٹ سنکنرن کے لیے بہت حساس ہوتے ہیں۔ لہذا ایک حفاظتی سطح کی کوٹنگ کی ضرورت ہے. NdFeB مقناطیس کے استعمال مشروط ہیں۔
80ºC سے 230ºC تک چلنے والی وسیع رینج میں درجہ حرارت کے ذریعہ۔ اور یہ 0 ℃ سے کم درجہ حرارت پر بھی کام کرتا ہے۔
درخواست:
نیوڈیمیم میگنےٹ کو مختلف قسم کے مقناطیسی لینز کے طور پر فوکس کرنے، الیکٹرانکس میں چارج شدہ ذرات کے انحراف، بریک سسٹم،
ڈرپ، سینسر، روٹر اور مائیکرو موٹرز میں مقناطیسی نظام، اور سائنس کا شعبہ، طب (ٹوموگرافی، این ایم آر سپیکٹرو میٹر) وغیرہ۔
آج، پوری دنیا میں NdFeB میگنےٹ بڑی مقدار میں استعمال ہوتے ہیں۔ اس مواد کی ترقی ابھی مکمل نہیں ہوئی ہے۔ بقایا
اور زبردستی فیلڈ کی طاقت میں مسلسل اضافہ کیا جا رہا ہے۔ NdFeB میگنےٹس کی اعلی توانائی کا مطلب ہے کہ موٹرز اور سینسر بنائے جا سکتے ہیں۔
کبھی چھوٹا - اور یہ کارکردگی کی کارکردگی میں اضافے کی نشاندہی کرتا ہے۔ جاری بہتری اس دلچسپ مواد کو جاری رکھنے کے قابل بناتی ہے۔
عام طور پر نئے علاقوں میں متعارف کرایا جاتا ہے۔
تمام بیان کردہ قدروں کا تعین IEC 60404-5 کے مطابق معیاری نمونوں کے ذریعے کیا گیا تھا۔ مندرجہ ذیل وضاحتیں حوالہ اقدار کے طور پر کام کرتی ہیں اور
مختلف ہو سکتے ہیں. مزید معلومات کے لیے براہ کرم ہمارے ایپلیکیشن انجینئرز سے رابطہ کریں۔